Study on the dynamic fracture behavior and energy consumption characteristics of granite with a pre-cut mode-I crack under impact loading

PLOS ONE
CC BY
이 매체는 공공·자유 라이선스로 본문을 직접 표시합니다.

Figures
Abstract
To investigate the dynamic fracture behavior and energy consumption characteristics of granite containing pre-cut mode-I cracks of different sizes under impact loading, split Hopkinson pressure bar (SHPB) tests are conducted on Brazilian disc specimens with four height-to-diameter (H/D) ratios. The results show that the deformation and failure process of pre-cracked granite can be divided into three stages: linear elastic deformation, plastic yielding, and post-peak failure. Both peak stress and fracture toughness exhibit an exponential increase with average strain rate, with the strongest strain-rate sensitivity observed for H/D = 0.1. Increasing the H/D ratio enhances peak stress and fracture toughness, whereas higher strain rates weaken this size effect. The cracking process is dominated by mode-I failure. Impact pressure enlarges the crushing zones and increases the degree of fragmentation, but damage extent decreases with increasing H/D ratio, leading to improved specimen integrity. The reflected, transmitted, and absorbed energies all increase with incident energy, and the absorbed energy exhibits significant strain-rate and size effects. The specific energy absorption (SEA) and mass-specific crushing energy consumption (Md) both increase exponentially with dynamic peak stress and fracture toughness.Specimens with H/D = 0.5 show the highest energy absorption capacity and require the most energy for fragmentation. The damage variable and dissipated energy evolution curves follow a “slow growth – rapid growth – approximately linear growth” pattern. Numerical simulations for H/D = 0.1 and 0.5 reproduce the observed size-dependent fracture patterns and energy partitioning, confirming that lateral confinement controls the size effect under diametral impact loading.
Citation: Wang Y, Hou Y, Wan M, Liu B, Li X, Li Y, et al. (2026) Study on the dynamic fracture behavior and energy consumption characteristics of granite with a pre-cut mode-I crack under impact loading. PLoS One 21(11): e0363058. https://doi.org/10.1371/journal.pone.0363058
Editor: Wislei Riuper Osório, UNICAMP, University of Campinas, BRAZIL
Received: June 5, 2026; Accepted: November 3, 2026; Published: November 25, 2026
Copyright: © 2026 Wang et al. This is an open access article distributed under the terms of the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original author and source are credited.
Data Availability: All raw experimental data required to replicate the findings of this study are available within the paper and its Supporting Information files.
Funding: This work was supported by the Science and Technology Basic Strengthening Program (Project No. 6142902210201), the National Natural Science Foundation of China (Grant Nos. 52504111, 42402287, 52504112), the Open Fund of Key Laboratory of Xinjiang Coal Resources Green Mining, Ministry of Education (KLXGY KB2605), the Anhui University of Science and Technology Research Startup Fund for Introduced Talents (2025yjrc0142), and the Open Fund of Anhui University of Science and Technology Engineering Laboratory for Safe and Precise Coal Mining (2024AH050394). The funders had no role in study design, data collection and analysis, decision to publish, or preparation of the manuscript.
Competing interests: The authors have read the journal’s policy and have the following competing interests: YanLi WANG, MingMing WAN, BoWen LIU, Xue LI, Yuan LI, and HengJun ZHANG are salaried employees of the No. 52 Institute of China North Industries Group Corporation Limited. YongQiang HOU is affiliated with Xinjiang Institute of Engineering and Anhui University of Science and Technology. The commercial affiliation of the authors with the No. 52 Institute of China North Industries Group Corporation Limited does not alter our adherence to PLOS ONE policies on sharing data and materials. The other authors have declared that no competing interests exist.
Introduction
Many geotechnical disasters,such as roadway roof failure, rockburst, and coal burst, are closely related to rock fracture [1,2]. During underground excavation, the surrounding rock mass is frequently subjected to dynamic loads from blasting and mechanical impact. The deformation and failure of rock under such conditions exhibit significant strain-rate effects, which alter fracture behavior and influence roadway stability [3]. Therefore, understanding the dynamic fracture behavior of rock, the energy transfer mechanisms, and the energy consumption characteristics during fragmentation is essential for stability analysis and safe excavation design [4,5].
Rock fracture has been extensively studied in rock mechanics. Previous research has examined the influence of loading rate on fracture toughness [6], stress intensity factors and crack propagation velocities under impact [7], depth-dependent fracture behavior of basalt [8]; low temperature and loading rate effects on frozen sandstone [9], fracture characteristics of layered composite rocks [10], loading rate effects on fracture toughness [11], temperature effects on granite fracture [12], impact velocity effects on surrounding rock fracture [13], fragmentation strength and energy consumption under impact [14], dynamic response of double-hole rock specimens [15], fractal characteristics and energy release patterns under impact [16],and natural joints effects on fracture and energy evolution [17]. These studies have yielded valuable insights; however, most focus on intact rock specimens. Similarly, the energy transfer characteristics of deep-mine marble [18] have been investigated, but the specific behavior of pre-cracked granite with controlled mode-I geometry remains unexplored..
Rock mechanical properties also exhibit significant size effects, which are critical for extrapolating laboratory results to engineering-scale rock masses [19]. Previous studies have investigated size effects on prefabricated cracked specimens under dynamic loading [20], length effects on dynamic compressive strength of limestone [21], triaxial size effects in siltstone [22], fragmentation energy consumption of rocks with different height-to-diameter ratios [23], and size effects in fractured rock masses [24]. However, most of thesestudies also focus on intact specimens or single-sized cracked geometries, and the combined effects of specimen size (H/D ratio) and strain rate on dynamic fracture toughness and energy dissipation of pre-cracked granite have not been systematically addressed.. Furthermore, the quantitative relationship between energy consumption parameters (SEA, Md) and mechanical properties (peak stress, fracture toughness) under impact loading remains insufficiently established.
To fill these gaps, this study systematically investigates the dynamic fracture behavior, energy dissipation, and size effects of granite specimens containing a central pre-cut mode-I crack under SHPB impact loading, using four H/D ratios (0.1, 0.2, 0.3, 0.5).The original contributions are: (1) simultaneous quantification of the strain-rate effect and size effect on mode-I fracture behavior of pre-cracked granite; (2) establishment of the correlation between energy absorption indices and dynamic strength/fracture toughness, revealing the underlying energy mechanism; (3) development of a damage constitutive model incorporating the H/D ratio, capable of predicting stress-strain response and damage evolution; and (4) numerical simulations for H/D = 0.1 and 0.5 that reproduce the experimental fracture patterns and energy partitioning, providing mechanistic insights into the size effect.This work offers a basis for extrapolating laboratory results to engineering-scale rock masses and contributes to the understanding of dynamic fracture in jointed rock under impact loading.
Materials and methods
Specimen preparation
The material used in this study was biotite granite, a pre‑existing laboratory specimen originally collected from the Beishan area, Gansu Province. To minimize the influence of mineral heterogeneity and anisotropy on the mechanical properties, all specimens were drilled from the same intact rock block in the same direction using a waterdrilling method. Central straight‑crack Brazilian disc (CSTBD) specimens were prepared for impact splitting tests to determine fracture toughness [25].
The specimens were processed using a fully automatic wire cutting machine.The rock block was fist fixed on the processing platform, and a numerical control program was developed to guide the cutting path. An abrasive wire with a diameter of approximately 0.6 mm was then used to cut the disc specimens according to the programmed geometry. The initial length of the central pre-cut crack was designed as 16.67 mm and its width as 1 mm, based on calculations referenced from existing studies on central straight-crack dimensions [26].After cutting, a diamond abrasive wire with a diameter of 0.3 mm was used to polish the crack tip until it met the requirements for fracture toughness testing.
The Brazilian disc specimens had a diameter of 50 mm. To investigate the influence of specimen size effects on rock fracture characteristics, four specimen heights were designed: 5 mm, 10 mm, 15 mm, and 25 mm, corresponding to height-to-diameter (H/D) ratios of 0.1, 0.2, 0.3, and 0.5, respectively. The prepared Brazilian disc specimens with different H/D ratios are shown in Fig 1 and 2.
Experimental setup and methods
A split Hopkinson pressure bar (SHPB) system with a bar diameter of 40 mm was used to conduct impact splitting tests on Brazilian disc specimens containing a central straight crack. The system consists of three main parts: the power system, the loading device, and the measurement system. The detailed parameters of the SHPB equipment are listed in Table 1.
To ensure stable contact between the specimen and the incident/transmission bars under high-speed impact loading, small flat surfaces with a width of approximately 2 mm were ground on both loading ends of the disc specimen using a surface grinder.Each granite Brazilian disc specimen wasplaced between the incident bar and transmission bar along the loading direction and then subjected to impact loading under different gas pressures. Four impact gas pressures, i.e.,0.1 MPa, 0.3 MPa, 0.4 MPa, and 0.6 MPa,were selected, corresponding to measured impact velocities of 12 m/s, 20 m/s, 25 m/s, and 32 m/s, respectively.
For rock fracture toughness testing, commonly used specimens include the center-cracked semi-circular disc, the center chevron-notched disc, and the center-cracked disc [27,28]. In this study, the center-cracked disc specimen was selected. The specimen was subjected to impact loading using the SHPB system to obtain the peak loading stress, from which the mode‑I and the mode‑II fracture stress intensity factors, KI and KII were derived. Their expressions are given as [29]:
(1)(2)where: is the peak stress, is the half-crack length, R is the radius of the specimen, B is the thickness of the specimen, and are two dimensionless coefficients that depend on the specimen geometry and the loading direction in the mechanical test. Their specific calculation formulas are as follows:
(3)(4)where: , , and ,whose calculation formulas are given as follows:
(5)(6)(7)where: represents the angle between the loading direction and the crack orientation.The calculation formulas for coefficients and are as follows:
(8)(9)(10)(11)Based on the formulas above, it can be calculated that when ,,,corresponding to pure mode‑I loading; When ,,corresponding to pure mode‑II loading. Therefore, in this experiment, the angle between the crack and the loading direction in the center-cracked disc specimen was varied to analyze the fracture behavior of granite with a pre-cut mode‑I crack under impact loading. The SHPB test system is shown in Fig 3.
To ensure statistical reliability, each impact condition (combination of H/D ratio and impact pressure) was repeated at least three times, and the average values of peak stress, fracture toughness, and energy parameters were used for analysis. The standard deviations were calculated and are presented as error bars in the corresponding figures (Figs 4–7).
Principles of SHPB impact testing
The objective of this experiment is to investigate the dynamic mechanical properties of granite with a pre-cut mode-I crack under impact loading. Prior to loading, couplant was applied between the specimen and the bar end faces to ensure full contact between the rock specimen and the bars. Based on one‑dimensional stress‑wave theory and the assumption of stress equilibrium, the following analytical relationships are used to determine the strain, strain rate, and stress in the specimen as functions of time [30]:
(12)(13)(14)In the above equations: A is the cross‑sectional area of the bar; is the cross‑sectional area of the specimen; is the elastic modulus of the pressure bars; is the thickness of the specimen; C0 is the velocity of the elastic stress wave; is the reflected strain; is the transmitted strain; is the dynamic stress in the specimen; is the strain rate of the specimen; is the strain of the specimen.
No field‑site permits were required for this study. All experiments and sample preparation were performed under laboratory conditions. No field sampling, field investigation or access to protected land sites was involved in this work. The biotite granite rock blocks used in this study were pre‑existing laboratory specimens originally collected from the Beishan area, Gansu Province.
Results and discussion
Stress-strain curve features of granite with a pre-cut crack
The SHPB system was used to apply impact loading to specimens with different H/D ratios. Fig 8 presents the stress-strain curves of granite with a pre-cut mode-I crack under impact loading. As shown, all curves exhibit a similar trend: the stress increases rapidly with strain initially, followed by a significant decline, indicating that the failure mechanisms are essentially similar for all H/D ratios and impact intensities.
As shown in Fig 8(d), the deformation and failure process can be divided into three stages: the linear elastic deformation (OA), plastic yielding (AB), and post-peak failure (BC).
For specimens of the same dimensions, the linear elastic stage extends to higher stress levels with increasing strain rate, indicating a pronounced strain-rate effect On yield stress. Under a constant impact intensity, although the overall shape of the stress-strain curves remains similar, the linear elastic stage extends to higher stress levels as the H/D ratio increases, revealing a significant size effect on yield stress.
Peak stress response in granite with a pre-cut crack
Impact loading tests were conducted on granite specimens with a pre-cut mode-I crack. The peak stresses of specimens with different H/D ratios are presented in Fig 4.
As shown in Fig 4(a), the peak stress increases exponentially with the average strain rate for all H/D ratios, and the specimens with H/D = 0.1 exhibit the most pronounced strain-rate sensitivity. Under impact loading, the extremely short loading duration prevents the absorbed energy from dissipating in time; consequently, energy accumulates within the specimen, extending the linear elastic deformation stage to higher stress levels and thereby enhancing the peak stress [31].
Fig 4(b) indicates a positive linear correlation between peak stress and H/D ratio, suggesting that a larger H/D ratio significantly enhances peak stress and demonstrates a clear size effect. However, the slope of this correlation decreases with increasing strain rate, indicating that the size effect is attenuated at high strain rates. This attenuation can be attributed to the shorter loading duration at higher strain rates, which reduces the time available for stress wave propagation and thus diminishes the influence of specimen geometry on the mechanical response. Under impact loading, specimens with larger H/D ratios require more energy for the initiation, propagation, and coalescence of internal cracks; as a result, they exhibit higher yield strength, leading to increased peak stress [32].
The underlying mechanism for this size-dependent peak stress behavior can be understood from stress wave dynamics. Under diametral impact loading, the H/D ratio controls the distance between the two free circular faces of the Brazilian disc and the central crack plane. For thin specimens (H/D = 0.1), stress waves reflected from these free faces return to the loading ends and crack tip within a very short time, superimposing with the incident wave and creating complex tensile–compressive stress states that promote premature local crushing. This consumes a substantial portion of the input energy before the specimen can sustain higher load. In contrast, for thick specimens (H/D = 0.5), the increased thickness delays the arrival of reflected waves and attenuates their amplitude, resulting in more uniform stress distribution and more efficient energy transfer to the central crack, thereby enhancing the peak stress. This mechanistic interpretation is further validated by the numerical simulations.
Variation in fracture toughness of granite with a pre-cut crack
The fracture toughness values of granite specimens with different H/D ratios were calculated using the formulas (1), and the results are shown in Fig 5. Under impact loading, the fracture toughness increases with both the average strain rate and the H/D ratio, indicating distinct strain rate and size effects.
As shown in Fig 5(a), fracture toughness increase with average strain rate across all H/D ratios, mirroring the trend observed for peak stress (Fig 4(a)). Specifically, as the average strain rate increases from approximately 85–90 s−1 to 570–586 s−1, the fracture toughness improves by 125.91%, 106.63%, 139.61%, and 150.79% for H/D ratios of 0.1, 0.2, 0.3, and 0.5, respectively. The magnitude of this enhancement generally increases with the H/D ratio, suggesting that larger specimens amplify the strain-rate sensitivity of fracture toughness.
Fig 5(b) shows that under different average strain rates, the fracture toughness also increases approximately linearly with the H/D ratio. This confirms a significant size effect on fracture toughness. Under impact loading, specimens with larger H/D ratios require more energy for crack initiation, propagation, and coalescence, which results in higher fracture toughness [33]. When the average strain rates are 88.31 s−1, 141.56 s−1, 387.22 s−1, and 577.88 s−1, the fracture toughness increases by 57.43%, 61.25%, 96.62%, and 74.77%, respectively, as the H/D ratio rises from 0.1 to 0.5. It can be observed that the increase in fracture toughness first rises and then declines with increasing average strain rate. This indicates the existence of a strain-rate threshold for the size effect on fracture toughness:. below this threshold, the size effect is relatively pronounced, whereas above it, the size effect gradually diminishes. Based on the present data, this threshold lies between 387 s−1 and 578 s−1; its exact value requires further experimentaldetermination.
The size effect on fracture toughness can be similarly interpreted from the perspective of energy availability at the crack tip. For a given incident energy, specimens with larger H/D ratios absorb a greater proportion of energy, and this absorbed energy is more efficiently delivered to the pre-cut crack tip rather than being dissipated in end-crushing zones. The higher energy flux at the crack tip promotes more stable crack initiation and propagation, which macroscopically manifests as increased fracture toughness. Furthermore, the observed strain-rate threshold for the size effect (between 387 s−1 and 578 s−1) suggests that at very high strain rates, the loading duration becomes so short that stress wave reflections from free faces have insufficient time to return and interfere with the main crack propagation, thereby attenuating the geometric influence. This dynamic shielding mechanism explains why the size effect diminishes beyond a critical strain rate.
Fracture evolution characteristics of granite with a pre-cut crack
A high-speed camera was used to capture the dynamic fracture process of granite Brazilian disc specimens with a central straight crack under various impact intensities. Fig 9 shows the dynamic fracture process of specimens with H/D = 0.5 under different average strain rates. As illustrated, the primary fracture surface aligns with the plane of the pre-existing crack, and the cracking process exhibits a typical mode-I failure morphology. Localized stress concentration at the two loading ends leads to the formation of triangular crushing zones. with the zone at the incident bar end generally larger than that at the transmission bar end.
The size of the crushing zones and the degree of fragmentation increase with rising impact pressure. This is attributed to the large elastic modulus mismatch between the bars and the rock specimen, which causes incompatible deformation at the contact interfaces. The resulting stress concentration intensifies with increasing impact pressure, leading to localized compressive failure at the specimen ends before the central pre-cut crack becomes unstable and propagates.
In addition, under mode-I loading at different impact pressures, multiple secondary cracks consistently develop parallel to the pre-cut crack. As the impact pressure increases, the number of secondary cracks grows, and their propagation eventually forms new fracture surfaces. Stress concentration occurs not only at the pre-cut crack tip but also at other microscopic flaws within the specimen. Under dynamic impact, these micro-cracks also initiate; their propagation and coalescence generate macroscopic secondary cracks, ultimately leading to multi-directional fracture failure of the specimen [33].
Fig 10 illustrates the dynamic fracture characteristics of granite specimens with different H/D ratios under an impact pressure of 0.3 MPa. The fracture patterns vary significantly with the H/D ratios, indicating a strong influence of specimen size on fracture morphology.
For H/D = 0.1, the specimen breaks into irregularly small fragments and loses its original shape, exhibiting the most severe fragmentation. For H/D = 0.2, the specimen also fractures noticeably, with larger fragment sizes H/D = 0.1 case, but it still cannot maintain a complete form. As the H/D ratio increases to 0.3 and 0.5, the specimens fail under impact loading but break into larger blocks; notably, specimens with a H/D = 0.5 retain relatively high integrity.
Therefore, as the H/D ratio increases, the degree of damage in the granite specimens decreases, and the specimen integrity progressively improves. This trend is macroscopically reflected in the continuous increase in peak stress.
Numerical simulation of dynamic fracture behavior
To further elucidate the mechanisms underlying the observed size effect and fracture evolution, numerical simulations were performed for granite specimens with H/D ratios of 0.1 and 0.5 under impact loading. The simulations employed LS-DYNA, which has been widely used to model rock dynamic fracture. The primary objective was to reproduce the experimentally observed differences in fracture morphology and energy partition between thin and thick specimens, thereby providing mechanistic insights into the size effect.
Model setup.
The numerical model replicated the Brazilian disc specimen with a central pre-cut crack, with dimensions identical to those in the experiments: diameter 50 mm, thickness 5 mm for H/D = 0.1 and 25 mm for H/D = 0.5. The granite was modeled using the Holmquist–Johnson–Cook (HJC) constitutive model, which is widely employed for rock-like materials subjected to high strain rate and high-pressure loading. The HJC model incorporates pressure-dependent strength, strain rate effects, and cumulative damage evolution, making it suitable for simulating the dynamic fracture behavior of granite under SHPB impact.
The normalized equivalent stress in the HJC model is expressed as:
(15)Where =σ/ is the normalized equivalent stress, =P/ is the normalized hydrostatic pressure, =/ is the dimensionless strain rate (with =1.0 s−1), D is the damage variable (0 ≤ D ≤ 1), and A, B, N, C, and Smax are material constants. The parameter Smax represents the maximum normalized equivalent stress that the material can achieve.
The pressure–volume relationship is described by a three-stage equation of state. The elastic stage is governed by the bulk modulus K, while the transition and compaction stages are defined by the parameters K1, K2, K3, Pcrush, μcrush, Plock, and μlock. Damage accumulation is controlled by the equivalent plastic strain and plastic volumetric strain, with the damage parameters D1, D2, and the minimum fracture strain EFMIN.
The material parameters adopted in the simulation are listed in Table 2, and were calibrated based on the quasi-static and dynamic mechanical properties of the tested granite. In particular, the density was ρ = 2600 kg/m3, the uniaxial compressive strength =144.8 MPa, the shear modulus G = 11.85GPa, and the tensile strength T = 3.2MPa. The pre-existing crack was represented by a zero-thickness cohesive interface, and crack propagation was governed by an element erosion technique consistent with the damage evolution of the HJC model.
In the simulation, the loading direction was along the diameter of the disc, with the incident bar contacting the circumferential surface of the specimen, while the two flat circular faces remained free, consistent with the experimental setup. The incident stress wave was applied at the end of the incident bar with the same amplitude and duration as in the experiments, corresponding to impact velocities of 20 m/s (gas pressures of 0.3 MPa).
Comparison of fracture patterns with experiments.
Fig 11 shows the simulated crack propagation sequences for H/D = 0.1 and 0.5 at an impact velocity of 20 m/s, alongside the corresponding experimental images from Section 2.4. For both configurations, damage initiates near the impacted end at approximately 6us. Driven by the transmitted stress waves, primary cracks originate from the pre-cut tip and propagate towards the free boundary.Secondary branching cracks gradually emerge as time increases from 12us to 54us, accompanied by extensive diffuse damage zones.
Distinct differences in fracture patterns are observed between the two H/D configurations. For H/D = 0.1, failure is dominated by a single rapidly-propagating main tensile crack with limited secondary branching. In contrast, the specimen with H/D = 0.5 exhibits intensive multi- branching cracks and highly fragmented damage morphology.
It should be acknowledged that the numerical simulation for H/D = 0.1 did not fully reproduce the extensive fragmentation observed in the experiments (Fig 10). The experimental specimen disintegrated into multiple irregular small fragments, whereas the simulated specimen primarily broke into two major blocks with localized crushing zones. This discrepancy is not merely a modeling artifact but rather reveals an intrinsic limitation of the HJC continuum damage model: it cannot capture the random nucleation, growth, and coalescence of multiple microcracks that dominate the fragmentation process in thin specimens under high strain rates. The homogeneous continuum assumption inherently suppresses the stochastic heterogeneity that is essential for multi-crack branching and block formation. Additionally, the simplified axisymmetric geometry neglects out-of-plane stress wave reflections and local three-dimensional stress concentrations, which are particularly significant for thin specimens.
Despite this limitation, the numerical simulation successfully reproduces the key features governing the size effect, including more severe end crushing, lower energy absorption, and a higher reflected energy ratio for H/D = 0.1 compared with H/D = 0.5. The model captures the dominant crack path, stress concentration features, and energy partitioning trends that are the essential factors controlling the thickness-dependent fracture behavior. Therefore, the model is considered adequate for revealing the underlying mechanism of the size effect at the macroscopic scale. To fully reproduce the fine fragmentation process of thin specimens, future work should employ discrete element methods (e.g., PFC) or cohesive zone models with random defect fields, which can better represent the discontinuous nature of rock fragmentation under dynamic loading.
Stress wave propagation and energy partition.
In the Brazilian disc test, the incident stress wave propagates along the loading diameter, while the two flat circular faces of the disc remain free. The simulated stress field evolution reveals that for thin specimens (H/D = 0.1), the stress wave reflections from these free faces occur rapidly and repeatedly, resulting in strong localized stress concentration near the loading ends and premature crushing before the central crack can fully propagate. The transmitted stress wave amplitude is low, indicating that a significant portion of incident energy is reflected back. For H/D = 0.5, the increased thickness delays the arrival of reflected waves at the crack tip and attenuates their amplitude due to the longer propagation path along the transverse direction. This leads to a more uniform stress distribution, delayed crack initiation, and a more efficient transfer of energy to the central crack, which is consistent with the higher peak stress and fracture toughness observed experimentally.
Mechanism of size effect under diametral impact loading.
The numerical simulation provides a mechanistic explanation for the experimental observations. Under the diametral loading configuration of the Brazilian disc, the H/D ratio controls the degree of lateral confinement in the direction perpendicular to the loading diameter. For thin specimens (H/D = 0.1), the two free circular faces are close to the central crack and the loading ends. Stress waves reflected from these free faces superimpose with the incident wave, creating complex tensile–compressive stress states and promoting crack branching and fragmentation. The high stress concentration at the loading ends causes severe local crushing, consuming a large portion of the input energy before the central crack can propagate. Consequently, the peak stress, fracture toughness, and absorbed energy are relatively low.
In contrast, for thick specimens (H/D = 0.5), the lateral free faces are farther from the crack tip, so the reflected waves arrive later and with reduced amplitude. The enhanced lateral confinement suppresses premature crack branching and allows the main crack to propagate stably along the pre-existing crack plane. More energy is thus transferred to the crack tip, resulting in higher peak stress, fracture toughness, and absorbed energy. This mechanism is further supported by the simulated energy partition: the reflected energy ratio decreases with increasing H/D, indicating more efficient utilization of incident energy for fracture.
Although the simulation does not fully replicate the fine fragmentation of thin specimens, it successfully reproduces the dominant fracture mode, stress concentration features, and energy partitioning trends, which are the key factors governing the size effect. These results validate the experimental findings and provide a clear physical interpretation of the observed size dependence.
Energy evolution characteristics of granite with a pre-cut mode‑I crack under impact loading
Energy values of granite with a pre-cut mode‑I crack under impact loading.
Under impact loading, the deformation and failure of granite with a pre-cut mode‑I crack are accompanied by energy transformations. The relationship among the incident energy (WI), reflected energy (WR), transmitted energy (WT), and absorbed energy (WS) of the specimen is given as [34]:
(16)(17)(18)(19)In the above equation, WI represents the incident energy of the specimen, WR is the reflected energy, WT is the transmitted energy, and WS is the absorbed energy by the specimen.
Following the method for characterizing absorbed energy per unit volume of the specimen, the specific energy absorption (SEA) is introduced to represent the absorbed energy per unit volume of the granite specimen. Its calculation formula is given by Equation (20) as follows:
(20)In the above equation, WS is the absorbed energy of the specimen (unit: J), and VS is the volume of the specimen (unit: cm³).
Meanwhile, to quantitatively analyze the energy dissipation characteristics of granite, the mass-specific energy absorption for crushing Md is introduced, defined as the energy absorbed per unit mass required for fragmentation [35]:
(21)In the above equation: Md is the crushing energy consumption per unit mass of the specimen(unit: J/g); WS is the absorbed energy of the specimen(unit: J); MS is the mass of the specimen(unit: g).Based on the above energy calculation formulas, the energy values during the dynamic impact process of granite with a pre-cut mode‑I crack were calculated. The calculation results are presented in Table 3.
Variation characteristics of reflected, transmitted, and absorbed energy with incident energy.
Based on the energy calculation results in Table 3, the relationships between incident energy and reflected, transmitted, and absorbed energy are plotted in Fig 6. As shown, the reflected, transmitted, and absorbed energy of granite specimens with pre-cut mode‑I crack all increase with rising incident energy, and the absorbed energy exhibits a clear correlation with the H/D ratio.
The proportion of reflected energy for each H/D ratio at different average strain rates was calculated from the data in Table 3. For H/D = 0.1, the reflected energy ratio increases from 89.91% to 97.41% as the average strain rate rises from 90.21 s−1 to 585.81 s−1, and remains above 96% at higher strain rates. For H/D = 0.2, the ratio increases from 80.08% to 94.37% with increasing strain rate, then slightly decreases to 92.59% at 575.98 s−1. For H/D = 0.3, the ratio rises from 69.29% to 90.85%, then slightly decreases to 88.71% at 581.75 s−1. For H/D = 0.5, the ratio increases from 49.55% to 82.86%, then decreases to 79.17% at 567.98 s−1.
These results indicate that that under impact loading, the proportions of transmitted and absorbed energy are relatively small, and most of the incident energy is dissipated in the form of reflected energy. In addition, the proportion of reflected energy generally increases with increasing average strain rate, whereas for a given strain rate, it decreases with increasing H/D ratio. This suggests that larger specimens convert a greater proportion of incident energy into absorbed energy, demonstrating a clear size-dependent energy partitioning behavior.
The dominance of reflected energy can be explained by the acoustic impedance mismatch between the steel bars and the granite specimen. The reflection coefficient for a plane wave at the bar–specimen interface is given by
(22)where Z= is the acoustic impedance. For granite with ≈2600 kg/m3 and C ≈ 4000m/s, and for the steel bar with ≈7800 kg/m3 and C ≈ 5100m/s, the theoretical reflection coefficient is approximately 0.59. However, the measured reflected‑energy ratios frequently exceed 0.9, indicating that additional energy‑loss mechanisms, such as interfacial friction and microcrack closure, also contribute to the energy partitioning at the specimen‑bar interface.
As the H/D ratio increases, the effective acoustic impedance of the specimen becomes closer to that of the bar, which reduces the reflection coefficient and increases the fractions of transmitted and absorbed energy. This explains why specimens with H/D = 0.5 exhibit the high absorbed energy and the minimum reflected‑energy ratio among all tested samples.
A linear regression between the reflected‑energy ratio RE and the H/D ratio under a fixed strain rate yields RE = 0.98–0.72(H/D) with R2 > 0.95, quantitatively confirming the size effect on energy partitioning during dynamic loading.
To further quantify the geometric effect on energy partitioning, we examine the absorbed energy ratio (WS/WI) across different H/D ratios. At the highest strain rate (approximately 570–586 s−1), the absorbed energy ratio increases from 3.28% for H/D = 0.1 to 20.41% for H/D = 0.5, a more than six-fold increase. In absolute terms, the absorbed energy for H/D = 0.5 (227.2 J) is 6.8 times that for H/D = 0.1 (33.2 J) under comparable incident energy (≈1110 J), despite the volume of the H/D = 0.5 specimen being only 5 times larger. This disproportionate increase (6.8 × vs. 5× in volume) indicates that the improvement in energy absorption efficiency is not merely a volume effect, but reflects a genuine geometry-dependent enhancement in energy utilization.
The physical origin of this disproportionate enhancement lies in the competition between two energy dissipation channels: end-zone crushing and main-crack propagation. For thin specimens, the early arrival of reflected waves from the free faces creates intense stress concentrations at the loading ends, leading to extensive end crushing that consumes energy without contributing to fracture toughness. As the H/D ratio increases, the delayed and attenuated reflections reduce end-zone energy dissipation, allowing a larger fraction of the absorbed energy to be channeled into main-crack propagation. This is evidenced by the fracture morphologies in Fig 10: H/D = 0.1 specimens disintegrate into small fragments with large crushed areas, while H/D = 0.5 specimens retain high integrity with a single dominant fracture surface. The energy efficiency of fragmentation, defined as the ratio of fracture surface energy to total absorbed energy, thus improves substantially with increasing H/D ratio.
Correlation of energy absorption indices with dynamic mechanical properties.
Under impact loading, the relationship between dynamic peak stress, fracture toughness, and the energy absorption indices SEA (specific energy absorption) and Md(mass-specific crushing energy consumption) are presented in Fig 7. It reveals a consistent positive correlation between energy absorption capacity and dynamic mechanical properties. Notably, both SEA and increase exponentially with peak stress and fracture toughness, confirming that the energy dissipated during fracture is intrinsically linked to the specimen’s resistance to crack initiation and propagation.
Specifically, as the average strain rate increases from approximately 85–90 s−1 to 570–586 s−1, the SEA and increase by 849.51% and 848.57% for H/D = 0.1, 787.04% and 784.28% for H/D = 0.2, 675.76% and 677.17% for H/D = 0.3, and 619.25% and 621.27% for H/D = 0.5, respectively. The most pronounced increase occurs for specimens with H/D = 0.1, indicating a stronger strain-rate sensitivity of energy absorption in thinner specimens.
Furthermore, when the average strain rate is approximately constant, both the fracture toughness and the energy absorption indices increase with the H/D ratio. Specimens with H/D = 0.5 exhibit the highest fracture toughness and the greatest energy consumption for fragmentation, whereas specimens with H/D = 0.1 show the lowest values for all three parameters.
The underlying mechanism can be explained as follows. Under impact loading, the extremely short loading duration prevents internal cracks from initiating and propagating sufficiently to dissipate energy; therefore, the specimen responds by elevating its stress level, leading to a simultaneous increase in peak stress, fracture toughness, and absorbed energy. In addition, specimens with a larger H/D ratio require more energy for the initiation, propagation, and coalescence of internal cracks, which is macroscopically manifested as higher fracture toughness and greater energy absorption [36,37].
Energy damage evolution process of pre-cracked granite based on energy dissipation.
Under impact loading, the yield failure and damage of granite specimens are inevitably accompanied by energy dissipation, which is closely related to the progressive degradation of strength. The level of dissipated energy can be used to characterize the degree of damage in pre-cracked granite specimens during loading [18,38]. Accordingly, the damage variable D is defined as the ratio of cumulative dissipated energy to total dissipated energy, expressed as follows [38,39]:
(23)where: D is the damage variable; is the cumulative dissipated energy at time t(MJ/m3); and is the total dissipated energy (MJ/m³).
Based on the shape of the stress-strain curve of the granite specimen, it can be observed that after the impact test, the stress value of the specimen does not drop to zero. Therefore, a critical damage value Du is introduced to modify the damage variable:
(24)The critical damage value is calculated as [40]:
(25)Where is the residual stress after the test (MPa) and is the peak stress (MPa). Substituting Equation (25) into Equation (24) yields:
(26)According to Lemaitre’s strain equivalence hypothesis, the uniaxial damage constitutive relation for the pre-cracked granite specimen is given by [41]:
(27)Furthermore, the elastic modulus of pre-cracked granite specimens exhibits a size effect and can be expressed as:
(28)Where 、 and are fitting coefficients dependent on the H/D ratio .Substituting Equation (28) into Equation (27), the damage constitutive relationship considering the size effect is obtained as:
(29)Finally, substituting Equation (26) into Equation (29) gives the complete damage constitutive model for pre-cracked granite under impact splitting with different H/D ratios:
(30)Using the constructed damage constitutive model, the stress-strain behavior of pre-cracked granite specimens with different H/D ratios was calculated. Taking the specimen with a H/D = 0.2 as an example, the theoretical and measured stress–strain curves are compared in Fig 12. The predicted curves generally agree with the experimental results, although minor discrepancies exist in both the pre-peak and post-peak stages.The theoretical peak stress values are slightly higher than the measured one, but the relative errors are within 10%, confirming that the energy-based damage constitutive model can accurately predict the stress response of pre-cracked granite under impact splitting.
Using the model, the evolution curves of the damage variable D, dissipated energy(Ud), and elastic strain energy(Ue) for different average strain rate (ASR) are plotted in Fig 13. The trends of D and dissipated energy are consistent: When the dissipated energy reaches its maximum, D also reaches its extreme value. Based on these trends, the energy damage evolution can be divided into three stages:
- (1) Slow growth stage of damage energy dissipation (Stage OA). The damage value does not exceed 0.2and increases slowly; dissipated energy remains small and nearly constant. The specimen is in the linear elastic deformation stage, but damage still initiates, indicating that the deformation is not perfectly elastic. During this stage, the elastic strain energy is calculated using the initial elastic modulus rather than the unloading modulus, which may lead to the elastic energy slightly exceeding total strain energy and a transient decrease in the damage value [18,42].
- (2) Rapid growth stage of damage energy dissipation (Stage AB). The damage value increases rapidly with strain, corresponding to the yield failure stage. The elastic strain energy curve flattens while dissipated energy grows quickly, indicating the development of new internal cracks and asignificant increase in damage.
- (3) Damage failure stage (Stage BC). The damage value increases approximately linealy with strain, corresponding tothe post-peak failure stage. Elastic strain energy drops sharply while dissipated energy continues to rise linearly. When the damage value reaches itsmaximum, internal cracks have fully propagated and coalesced, leading to complete failure of the specimen under impact splitting.
Overall, during the entire impact deformation and failure process, the damage variable D and dissipated energy exhibit a characteristic pattern of “slow growth – rapid growth – approximately linear growth.”
Implications for engineering practice.
The experimental and numerical findings of this study have direct practical implications for underground excavation and dynamic disaster prevention:
Blast design optimization: The quantitative relationships between energy absorption indices (SEA, Md) and dynamic peak stress/fracture toughness provide a basis for calibrating blast efficiency models. For a given rock mass with known joint spacing (which effectively determines the characteristic block size, i.e., the effective H/D ratio), the required specific charge (explosive consumption per unit volume or mass) can be adjusted according to the Md values reported in Table 3. Specifically, for massive rock masses with larger effective H/D ratios, higher energy input is required to achieve the same degree of fragmentation, whereas thinly laminated or highly jointed rock masses (small effective H/D) may fragment more readily but with lower energy efficiency. This supports the optimization of charge weight and borehole spacing to reduce overbreak and improve fragmentation uniformity.
Excavation damage zone (EDZ) assessment: The H/D-dependent damage constitutive model (Equation 28) can be incorporated into numerical codes for predicting the extent of excavation damage under dynamic disturbance. The model captures the coupled effects of strain rate and geometry on stress–strain response, enabling more accurate estimation of the plastic zone radius around blast-excavated tunnels. When combined with the energy-based damage evolution criterion (Section 3.4), the model also provides a means to assess the progression of damage from initial microcracking to macroscopic failure, aiding in the evaluation of rockburst potential.
Rockburst and dynamic hazard mitigation: The finding that larger H/D ratios enhance energy absorption capacity has important implications for rockburst prevention. In deep mining where rockbursts are triggered by dynamic stress waves, rock masses with unfavorable geometry (e.g., thin slabs or plates) are more susceptible to dynamic failure because they reflect a larger portion of incident energy and absorb less energy before fracturing. This suggests that reinforcement measures (e.g., rockbolting or shotcreting) should be preferentially applied in zones where the rock mass exhibits low effective H/D ratios, as these zones have lower energy absorption capacity and higher failure susceptibility under dynamic loading.
Scaling from laboratory to field: The strain-rate threshold for the size effect (387–578 s−1) identified in this study provides a guideline for laboratory-to-field extrapolation. At strain rates above this threshold, the size effect becomes less pronounced, meaning that laboratory-derived fracture parameters from small specimens may be more directly applicable to field-scale rock masses under high-rate loading conditions (e.g., blasting). Conversely, at lower strain rates (e.g., seismic or tremor loading), the size effect must be carefully accounted for when scaling up laboratory results.
Conclusions
This study systematically investigated the dynamic fracture behavior, energy dissipation, and size effects of granite specimens containing a pre-cut mode-I crack under SHPB impact loading. The main conclusions and their engineering implications are as follows:
- (1) The deformation and failure of pre-cracked granite under impact loading exhibit three distinct stages (linear elastic, plastic yielding, and post-peak failure). Both peak stress and fracture toughness increase exponentially with average strain rate and increase approximately linearly with H/D ratio, demonstrating significant strain-rate sensitivity and size effects. A strain-rate threshold (387–578 s−1) exists beyond which the size effect on fracture toughness diminishes.
- (2) The size effect originates from stress wave propagation and reflection within the specimen, as revealed by LS-DYNA simulations. Larger H/D ratios delay and attenuate reflected waves from free faces, enhancing lateral confinement and promoting more efficient energy transfer to the crack tip. This mechanism explains the observed increases in peak stress, fracture toughness, and energy absorption with increasing H/D ratio.
- (3) Energy partitioning is dominated by reflected energy due to the acoustic impedance mismatch between steel bars and granite; however, the absorbed energy ratio increases with H/D ratio. The specific energy absorption (SEA) and mass-specific energy consumption (Md) both increase exponentially with dynamic peak stress and fracture toughness, with H/D = 0.5 specimens exhibiting the highest energy absorption capacity and fragmentation energy consumption.
- (4) The proposed energy-based damage constitutive model, incorporating the H/D ratio, effectively predicts the stress-strain response and damage evolution of pre-cracked granite under impact splitting. The damage variable and dissipated energy follow a “slow growth–rapid growth–approximately linear growth” pattern throughout the loading process.
- (5) These findings provide a basis for scaling laboratory fracture parameters to field-scale rock masses. The quantitative energy–strength relationships can inform blast design optimization, excavation damage zone assessment, and rockburst prevention strategies. The identified strain-rate threshold also offers a guideline for when size effects must be explicitly considered in laboratory-to-field extrapolation.
Supporting information
S1 File. Raw experimental data.
This file contains the minimal raw experimental data underlying the findings presented in this manuscript, including stress-strain data and fracture parameters of rock specimens.
https://doi.org/10.1371/journal.pone.0363058.s001
(ZIP)
References
- 1. Yao W, Wang J, Wu B, Xu Y, Xia K. Dynamic mode II fracture toughness of rocks subjected to various in situ stress conditions. Rock Mech Rock Eng. 2022;56(3):2293–310.
- 2. Cen D, Li Y. Frost heave cracking and uniaxial compression failure behavior of sandstone samples containing a flaw filled with water. Sci Rep. 2024;14(1):28711. pmid:39567754
- 3. Zhang JF, Xu RP, Liu Y. Study on micro–pore evolution law and shear mechanical behavior of grouting fractured rock mass under freeze-thaw cycle. Chin J Rock Mech Eng. 2022;41(4):676–90.
- 4. Liu K, Wang T. Dynamic mechanical behaviours of frozen rock under sub-zero temperatures and dynamic loads. International Journal of Rock Mechanics and Mining Sciences. 2024;180:105813.
- 5. Wang T, Jia H, Sun Q, Tan X, Tang L. Effects of thawing-induced softening on fracture behaviors of frozen rock. Journal of Rock Mechanics and Geotechnical Engineering. 2024;16(3):979–89.
- 6. Li ZL, Wang QZ. Experimental research on effect of loading rate for dynamic fracture toughness of rock. Chin J Geotech Eng. 2006;28(16):2116–20.
- 7. Song YM, Xing TZ, Lyu XF. Fracture characteristics of granite with mode-I pre-crack at different loading rates. Rock Soil Mech. 2018;39(12):4369-4376,4384.
- 8. Zuo JP, Chai NB, Zhou HW. Investigation on failure behavior of basalt from different depths based on three-point bending mesoexperiments. Chin J Rock Mech Eng. 2013;32(4):689–95.
- 9. Zhao T, Cui Z, Jia HL. Characteristics of dynamic mode II fracture of frozen saturated sandstones under varying low temperatures and loading rates. Coal Geol Explor. 2025;53(4):191–202.
- 10. Li Y, Wang YB, Fu DR. Energy dissipation and fracture characteristics of composite layered rock under dynamic load. Chin J Eng. 2023;45(11):1833–46.
- 11. Fang SZ, Yang RS, Li WY. Investigation of dynamic fracture characteristics of frozen red sandstone using notched semi-circular bend method. Chin J Eng. 2023;45(10):1704–15.
- 12. Zhou L, Dong YQ, Zhu ZM. Influence of high temperature on micro and macro mechanical fracture characteristics of granite. J Cent South Univ (Sci Technol). 2022;53(4):1381–91.
- 13. Zhang MT, Fan JY, Yang W. Experimental study on dynamic fracture and fragmentation behavior of surrounding rock in salt cavern gas storage under impact loading. Eng Fract Mech. 2025;328:111559.
- 14. Qaedi Tabar M, Asadi P, Ashraf MJ. Strength, energy consumption, particle size distribution and fracture toughness in rock fragmentation under dynamic loading. Eng Fract Mech. 2025;324:111237.
- 15. Xiang GL, Tao M, Zhao R. Dynamic response and fracture characteristics of rock with double holes under impact loading. Theor Appl Fract Mech. 2025;139:105082.
- 16. Liu W, Liu Y, Wang C, Zhai M. Study of fractal characteristics and energy release in rocks under impact loading. KSCE Journal of Civil Engineering. 2025;29(5):100101.
- 17. Zuo T, Li XL, Wang JG. Insights into natural tuff as a building material: Effects of natural joints on fracture fractal characteristics and energy evolution of rocks under impact load. Eng Fail Anal. 2024;163:108584.
- 18. Wang J, Lei L, Liu Y, Yang Y, Huang Y. Fracture fractal and energy transfer characteristics of deep-mine marble under an impact load. Minerals. 2023;13(2):275.
- 19. Xie HP. Research review of the state key research development program of China: Deep rock mechanics and mining theory. J China Coal Soc. 2019;44(5):1283–305.
- 20. Zhang S, Yu BX, Wang F. Experimental study on dynamic fracture characteristics of different sizes of rock specimens with a crack. J Min Saf Eng. 2021;38(5):1045–54.
- 21. Ping Q, Zhang H, Su HP. Study on dynamic compression mechanical properties of limestone with different lengths. Chin J Rock Mech Eng. 2018;37(S2):3891–7.
- 22. Zhu QZ, Min ZZ, Wang YY. Study on the size effect of silty sandstone samples under conventional triaxial compression. Chin J Rock Mech Eng. 2019;38(S2):3296–303.
- 23. Zhou J, Zhao GM, Meng XR. Dynamic impact energy dissipation characteristics of granite with different height-diameter ratios. J Min Saf Eng. 2023;40(2):379–86.
- 24. Luo GL, Zhang K, Qi FF. Size effect and anisotropy of mechanical properties of fractured rock masses based on 3D printing. Rock Soil Mech. 2023;44(S1):107–16.
- 25. Fan XD, Li X, Tao M, et al. Study on mode I and mode II fracture characteristics of granite under different thermal shock process. Gold Sci Technol. 2021;29(6):834–42.
- 26. Liu HY, Kou SQ, Lindqvist P-A, Tang CA. Numerical modelling of the heterogeneous rock fracture process using various test techniques. Rock Mech Rock Engng. 2006;40(2):107–44.
- 27. Kuruppu MD, Obara Y, Ayatollahi MR, Chong KP, Funatsu T. ISRM-suggested method for determining the mode i static fracture toughness using semi-circular bend specimen. Rock Mech Rock Eng. 2013;47(1):267–74.
- 28. Fowell RJ. Suggested method for determining mode I fracture toughness using Cracked Chevron Notched Brazilian Disc (CCNBD) specimens. International Journal of Rock Mechanics and Mining Sciences & Geomechanics Abstracts. 1995;32(1):57–64.
- 29. Atkinson C, Smelser RE, Sanchez J. Combined mode fracture via the cracked Brazilian disk test. Int J Fract. 1982;18(4):279–91.
- 30. Lin DN, Chen SR. Experimental study on damage evolution law of rock under cyclical impact loadings. Chin J Rock Mech Eng. 2005;24(22):4094–8.
- 31. Gong FQ, Lu DH, Li XB. Toughness increasing or decreasing effect of hard rock fracture with pre-static loading under dynamic disturbance. Chin J Rock Mech Eng. 2014;33(9):1905–15.
- 32. Dai SH, Ma SL, Pan YS. Evaluation of mode I stress intensity factor of rock utilizing digital speckle correlation method. Chin J Rock Mech Eng. 2012;31(12):2501–7.
- 33. Yue ZW, Yang RS, Sun ZH. Simulation experiment of rock fracture containing inclined edge crack under impact load. J China Coal Soc. 2010;35(9):1456–60.
- 34. Zhang XS, Wen GC, Zhu ZM. Dynamic propagation characteristics of mode I crack in infilled jointed rock masses under impact load. Rock Soil Mech. 2024;45(2):396–406.
- 35. Lee D, Tippur H, Bogert P. Dynamic fracture of graphite/epoxy composites stiffened by buffer strips: An experimental study. Compos Struct. 2012;94:3538–45.
- 36. Avachat S, Zhou M. High-speed digital imaging and computational modeling of dynamic failure in composite structures subjected to underwater impulsive loads. International Journal of Impact Engineering. 2015;77:147–65.
- 37. Chen ZQ, Li TB, Chen GQ, et al. Experimental study on energy evolution of sandstone under different stress paths. Eng Mech. 2016;33(6):120–8.
- 38. Wang P, Xu JY, Fang XY. Energy dissipation and damage evolution analyses for the dynamic compression failure process of red-sandstone after freeze-thaw cycles. Eng Geol. 2017;221:104–13.
- 39. Qin GP, Liu WZ, Du ZW. Study on triaxial compression energy and damage evolution law of cemented backfill under the influence of temperature. J Min Saf Eng. 2025;42(6):1409–22.
- 40. Liu BX, Huang JL, Wang ZY. Study on damage evolution and acoustic emission character of coal-rock under uniaxial compression. Chin J Rock Mech Eng. 2009;28(S1):3234–8.
- 41. Liu WZ, Chen JT, Guo ZP. Mechanical properties and damage evolution of cemented coal gangue-fly ash backfill under uniaxial compression: Effects of different curing temperatures. Constr Build Mater. 2021;305:124820.
- 42. Gong FQ, Luo S, Li XB. Linear energy storage and dissipation rule of red sandstone materials during the tensile failure process. Chin J Rock Mech Eng. 2018;37(2):352–63.